GLAZING FAULTS

Hi Everybody,

Last week, I did a blog about what a glaze actually is, so this week, I’m going to run through some of the common faults that can occur during the glazing process.

  • CRAZING: This is where hairline cracks appear on the surface of the glaze. The cause is a mismatch in the heat expansion between the clay body and the glaze: rapid cooling, cooling down too fast or the glaze is mixed incorrectly. The effects of this are that the clay body is weaker, and it can lead to staining and bacterial growth, not good!
  •  
  • Crawling: Another common fault, and it doesn’t mean crawling under the table, dragging yourself or slithering along. In ceramics, it’s when the glaze pulls away from the ceramic surface, leaving bare spots. The cause of this is often that the bisque surface has been contaminated with dust/oil/grease from your hands or the glaze may have been applied too thickly. The effect is that your pot will just look bloody awful and you might as well bin it!
  •  
  • Pin-holing: Not in any way related to Pinhead in the Hellraiser movie, but looks just as bad. It looks like lots of small holes or pits in the glaze surface. The cause of this is trapped gasses escaping from the clay body or the glaze during firing. This can occur if the kiln is fired too fast or, as often is the case, the glaze may be mixed incorrectly. Again, this just looks a mess, bin it and try again.
  •  
  • Blistering: Another glazing disaster. It looks like small, raised bumps on the glaze surface. Again this is the result of trapped air and is often caused by over-firing. Another cause can be that the glaze was applied too thickly or there is too much flux in the glaze (Flux, see last week’s blog.)
  •  
  • Shivering: This is where the glaze cracks and flakes off the clay body, often at the edges or rims. The glaze is mismatched with the glaze body, leading to detachment during the cooling process. Your pot will look like it has a disease, you know what to do!
  •  
  • Dunting: Actual cracks occur in the clay body and are visible through the glaze. The cause is rapid cooling and because the clay body may be cracked the pot could break.
  •  
  • Running: This is where the glaze runs/ melts too much during the firing and pools at the bottom of the pot. This is due to over-firing. If you’re lucky your pot will not have stuck to the kiln shelf, but is still probably un-savable!
  •  
  • Matte Glaze Defects: Here a matte glaze developed glossy spots or an uneven sheen. This is to do with variations in the firing temperature or the glaze has been applied unevenly. The appearance will not look good.
  •  
  • Peeling: The glaze entirely separates from the clay body and peels off in layers. The causes are poor glaze adhesion due to contaminants; the glaze could be incompatible with the clay body or there is an excessive shrinkage difference between the clay and the glaze. Whatever, your pot is ruined!
  •  
  • Glaze Fit Issues: This term basically covers everything mentioned above. The improper fit between glaze and the clay body or firing issues. I understand this may all sound a bit down-cast but if you know what glaze problems you have, you can try to rectify them.

Until next time,

Barry